This is the authors' abstract. We don't add key points for this paper.
The 2-powder method (2PM) for the production of high-performance Nd2Fe14B-based sintered magnets consists of blending a coarser heavy rare-earth (HRE) free main phase powder (here D50 = 5.3 µm) and a finer HRE-containing anisotropy powder (here D50 = 2.6 µm) of Dy content of 10 wt.%. The development of the core-shell structure was observed for different sintering conditions, namely at 1090°C for 5, 10, 30, 60, and 120 minutes. The diffusion behavior of the 2PM was investigated and the diffusion coefficient for the heavy rare-earth element dysprosium of D = (1.83 ± 0.54) x 10−11 cm2/s was determined. Magnets containing 0, 1, 2, and 3 wt.% Dy were produced by the 2PM and magnetic properties were analyzed in detail. A constant coercivity gain of around 120 kA/m per added Dy contents was reached. Dy was obtained without a significant decrease in remanence. Finally, the 2PM was compared with the conventional powder metallurgical production process. The enormous potential for decreasing the amount of critical HREs in Nd-Fe-B–based sintered magnets is demonstrated, especially in large volume magnets as 2PM is not restricted to 5 mm thick pieces, but can be applied to large scale.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Opelt et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: