A procedure is described to construct Kitagawa-Takahashi (K-T) diagrams to suit a given material and service load spectrum. The diagram serves as a graphic platform to audit permissible design stress level against desired service life and inspection period. It involves numerical analyses leading to a spectrum load S-N curve and residual fatigue crack growth estimates given initial defect size. The required analyses are performed on the Rainflow cycle count table for a given load spectrum. They account for potential load history effects on notch root fatigue crack initiation and near-threshold crack growth with and without crack closure. A key element of residual life estimates is consideration of sensitivity of threshold stress intensity range to load history in the absence of crack closure. The procedure was used to construct K-T diagrams for two aluminum alloys, a titanium alloy and a medium strength low alloy steel, subject to TWIST, HELIX, and TURBISTAN load spectra.
No takes yet. Share an insight, caveat, or question.
R. Sunder (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: