Answers are grounded in this paper and cite their sources.
ZrP 2 O 7 ceramics exhibit poor mechanical properties after firing, as a major drawback. In this study, ZrP 2 O 7 matrix composites reinforced with high silica fibers were prepared through pressureless sintering by varying the content and length‐to‐diameter ratio of the high silica fibers added to ZrP 2 O 7 powder. After heat treatment at 1200‒1300°C, the room temperature flexural strength of the ZrP 2 O 7 matrix composites with different amounts high silica fibers having different aspect ratios was 14.9‒45.2 MPa, the bulk density was 1.90‒3.03 g·cm −3 , the apparent porosity was 2.37%‒39.39%, and the room temperature thermal conductivity was .47‒.95 W/(m·K). With an increase in the heat‐treatment temperature, driven by sintering and fiber crystallization, strength of the interfacial layer between the fibers and the matrix inside the ZrP 2 O 7 matrix composites decreased and then increased. The transfer and blocking effects of the interface enabled effective transfer of the stress of the matrix to the fiber‐reinforced phase and prevented crack extension. The problem of inherent crystallization affecting high silica fibers at high temperatures was relieved by the ZrP 2 O 7 ceramic matrix composites.
No takes yet. Share an insight, caveat, or question.
Zhu et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: