Answers are grounded in this paper and cite their sources.
After multiple cycles of thin film deposition in the chip manufacturing process, steps will naturally occur, causing local or global protrusions and unevenness on the chip surface. This article introduces the phenomenon of local or global protrusions and unevenness on the wafer surface after deposition of silicon nitride thin films. The CF gas containing H and high argon gas volume flow rate are flattened under strong physical bombardment conditions using plasma plasma etching technology, and the silicon nitride thin film will stop at the designated position through a high selectivity etching process of silicon nitride on silicon dioxide.