In this study, a novel AA7075-TiO 2 metal matrix composite was machined utilizing a biosilica mixed EDM technique and the surface roughness and material removal rate are optimized. The biosilica particles are produced from waste maize cobs and then silane-treated. The optimization of process variables wasperformed using Taguchi grey relational approach with a process variable of peak current, gap voltage and pulse-on time. Results revealed that the gap voltage is the most important process variable, since it has a larger max-min difference of 0.25. In order to create a high MRR of 11.6[Formula: see text]mm 3 /min and a surface roughness of 2.25 m, the maximum GRG of 0.79 for Trial 1 (A2B1C3) represents the most ideal process variable group. The best results appear to be obtained with a peak current of 10 A, a gap voltage of 20[Formula: see text]V, and a pulse-on time of 140[Formula: see text][Formula: see text]s. The new GRG, however, is around 2.51% better than the anticipated optimized process variables of A2B1C3 with an old GRG of 0.79, according to the confirmation research. The new MRR of 11.89[Formula: see text]mm 3 /min and the surface roughness of 2.30[Formula: see text]s with a GRG of 0.81 are based on the optimized new process variables (A1B1C3).
No takes yet. Share an insight, caveat, or question.
Sakthimurugan et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: