Answers are grounded in this paper and cite their sources.
This study demonstrates the photocatalytic efficiency of NiO/PMMA films in dye degradation, highlighting optical and thermal properties.
This research employs the solution casting method to produce NiO/PMMA polymeric nanocomposite films, which are subsequently used to fabricate flexible photocatalytic membranes with varying nickel oxide nanoparticle (NiO NP) concentrations (0.25–3 wt%). XRD analysis confirmed the cubic structure of NiO, with the most intense (200) peak indicating a crystallite size of 19.42 nm. The Williamson–Hall method estimated the crystallite size to be 48.65 nm with a strain of 2.85 × 10 −3 . XPS results confirmed the presence of Ni +2 with characteristic Ni 2p 3/2 and Ni 2p 1/2 peaks at 856.55 and 874.94 eV, respectively. TGA revealed enhanced thermal stability, with 3 wt% NiO showing a decomposition temperature of 360.45°C. Optical studies revealed a redshift in the absorption edge and a decrease in the bandgap from 5.08 to 4.88 eV (direct) and from 4.77 to 4.46 eV (indirect). The lower band gap and higher optical constants of NiO/PMMA nanocomposites are correlated with the PL enhancement and redshift. Under UVC light, 3 wt% NiO/PMMA exhibited the highest MB dye degradation efficiency of 99.6% within 90 min. These nanocomposites demonstrate high potential for photocatalytic water purification.
No takes yet. Share an insight, caveat, or question.
Mohammed et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: