Answers are grounded in this paper and cite their sources.
Hydrothermal method improves glass quality using high-silica materials, indicating lower melting points.
The paper substantiates the possibility of expanding the raw material base of glass production through the use of high-silica raw materials, specifically tripoli. The essence of the study lies in the fact that the main glass-forming component, SiO2, is introduced at the expense of amorphous silica contained in tripoli. The charge was prepared using a hydrothermal method. Autoclave treatment of the fired mixture was carried out at 1500C for 10 hours under a pressure of 0.5 MPa in the presence of NaOH. The content of sodium hydroxide in the mixture for hydrothermal treatment was 25% calculated in terms of Na2O. Thermal analysis of the ordinary charge showed that dehydration reactions last up to 2000C, whereas for the hydrothermal charge dehydration occurs up to 5000C. This is explained by the release of chemically bound water from siloxane, silanol, and silandiol groups. For the ordinary charge, the next endothermic effect begins at 5000C and reaches its maximum at 5400C, which corresponds to the dehydration of kaolin and is 400C higher compared to the similar effect in the hydrothermal charge. In the ordinary charge, the following exothermic effects are observed at 6100C, 6500C, 8300C, and 9400C, which are associated with silicate formation. In contrast, for the hydrothermal charge, only two corresponding exothermic effects are recorded at 5800C and 8800C. Other exothermic effects occur at lower temperatures and overlap with the pronounced endothermic effect of water release from siloxane groups. XRD data confirm that the hydrothermal charge becomes almost completely amorphous at 10000C, and at 12000C all diffraction peaks disappear, indicating a fully glassy state. In the ordinary charge, even at 12000C, peaks corresponding to crystalline silica remain. Visual observation of the stages of glass formation revealed significant differences in the temperature intervals of silicate and glass formation between the hydrothermal and ordinary charges. The use of a hydrothermal charge allows the glass melting temperature to be reduced by 200–2500C.
No takes yet. Share an insight, caveat, or question.
Plemyannikov et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: