Hydrometallurgical synthesis produces pure zincite with 92.23% yield from waste batteries, indicating its potential for antimicrobial products.
The conversion of waste materials in our environment into useable chemical products is a popular issue these days. Here, we report on the production of zincite powder using a very simple hydrometallurgical method. Within two hours, 92.23% of the original 10 g/L SZCB reacted at ideal leaching conditions (2.5 mol/L HCl, 80°C). The result predicted the diffusion model as rate determining step, with calculated Ea of 28.53 kJ/mol. The precipitated hydroxide was calcined to produce pure zincite powder of yield 85.2%. Analyses using X-ray diffraction (XRD) and scanning electron microscopy (SEM) revealed that the high purity ZnO existed as a flower-like spherical aggregation and antimicrobial testing was later carried out to be reported in part B of the research.
No takes yet. Share an insight, caveat, or question.
A 2025 study studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: