Analysis demonstrates structural changes in tungsten microstructure after hydrogen plasma irradiation, suggesting impacts on durability.
The results of a study of the microstructure and structure of plates made of tungsten metal powder (group of companies “Specmetalmaster”, GC “SMM”) used as protective tiles in the lower divertor of the tokamak Globus-M and subjected to additional treatment with hydrogen plasma of a coaxial accelerator from distances of 50 and 260 mm at 5, 10 and 20 irradiation cycles are presented. The microstructure and elemental composition of the plate surface were determined by scanning electron microscopy and energy dispersive X-ray spectroscopy, respectively. The microstructure of the irradiated surface layer of the plates at a penetration depth of X-rays up to ~1.4 µm was analyzed from X-ray diffraction data using graphical methods of Williamson-Hall plot and crystallite size - microstrain plot adapted to take into account the observed pseudo-Voigt type of X-ray reflections. The structure of this layer was refined using the Rietveld method. The asymmetry of tungsten (W) reflections after plasma treatment was described by a model with 2 (for samples irradiated from a distance of 260 mm) and 3 (for a distance of 50 mm) crystalline W phases of the same cubic symmetry, but with slightly different parameters of the cubic unit cell and with different values of the mean size of crystallites and the absolute value of mean microstrain in them.
No takes yet. Share an insight, caveat, or question.
D D Polyakov (2025) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: