Contact angle tests show improved hydrophobicity and flotation recovery in sphalerite using a novel copper–amine activator, suggesting enhanced selectivity and sustainability.
Sphalerite (ZnS), the primary zinc-bearing mineral in most sulfide deposits, exhibits poor natural floatability and requires activation by metal ions such as Cu2+ or Pb2+. Copper sulfate (CuSO4) is the most common activator, but its use at high dosages introduces sulfate accumulation and necessitates separate pre-conditioning to prevent the formation of inactive copper xanthates. This study investigates a novel copper–amine complex, Zn Flooter (ZnFL), as an alternative activator for sphalerite flotation. ZnFL is a liquid reagent containing stabilized ionic copper with a significantly lower sulfate content. Contact angle and flotation tests were conducted on two sphalerite-bearing ores of different mineralogy (Pb–Zn and Cu–Zn types). Contact angle tests showed that ZnFL (68–71°) enhances sphalerite surface hydrophobicity more effectively than CuSO4 (61–66°). In flotation, ZnFL at 100 g/t achieved recoveries and grades comparable to those for CuSO4 at 500 g/t, while allowing simultaneous addition with the collector without loss of performance. ZnFL also exhibited improved sphalerite/pyrite selectivity and did not negatively affect froth stability. These results demonstrate that ZnFL can provide equivalent or superior activation efficiency at a lower dosage and with simplified operation. Further studies on adsorption mechanisms and water chemistry effects are recommended to validate its industrial potential as a sustainable activator for sphalerite flotation.
No takes yet. Share an insight, caveat, or question.
Bicak et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: