Understanding the strain effect in catalysis is vital for catalyst design but is complicated by the lack of model catalyst systems and strain-induced in situ reconstruction of the catalytically active phase. Here, we employ well-defined Pd-based model catalysts to thoroughly investigate how the surface strain impacts the oxygen reduction reaction (ORR). In contrast to the conventional expectation, Pd icosahedra (Pd-i) with a ∼2% tensile strain exhibit markedly enhanced catalytic stability toward the ORR compared to Pd octahedra (Pd-o). After 10 000 cycles of accelerated durability testing, Pd-i loses only 8.7% of its initial mass activity, while Pd-o suffers a 54.1% decline. Quasi-in situ spectroscopic characterizations and electrochemical analyses demonstrate that tensile strain in Pd-i promotes in situ hydrogen intercalation, leading to the formation of the PdHx active phase. In situ X-ray absorption spectroscopy and theory calculations reveal that H intercalation enhances the oxidation resistance of Pd and suppresses Pd dissolution by a strong Pd-H interaction.
No takes yet. Share an insight, caveat, or question.
Li et al. (2025) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: