Shows enhanced seawater electrolysis efficiency in green hydrogen production, suggesting a solution for anode durability.
Direct seawater electrolysis has potential in green hydrogen production; however, its anode is susceptible to chloride-induced corrosion, limiting its durability. Herein, using nickel foam (NF) as a catalyst support, we...