Assessment reveals enhanced hydrogen storage capacity of lignin pyrolyzed at 700°C, suggesting effective energy storage methods.
Due to their physicochemical properties, lignin deposits from black liquor treated through pyrolysis could be utilized as H2 storage. Density functional theory for H2 adsorption-desorption was assessed for lignin pyrolyzed at 400, 400,500, 600, 700, and 800°C, and its physicochemical properties were observed regarding porosity, morphology, metal contents, crystallinity, molecules within pyrolyzed lignin, surface characteristics, and hydrogen temperature-programmed desorption (H2 TPD). Most H2 was adsorbed on porous site with a large surface area for physisorption storage. Metals, as the physicochemical property detected on the surface of lignin by SEM-EDS, could increase the capacity of H2 storage since H is bound as a metal hydride. Pyrolyzed lignin at 700°C showed the highest porosity and H2 desorption, with 416.0558 m2 porous surface/g and 0.07221 thermal conductivity detector (TCD) signal (a.u.) area, respectively. However, to release H2 bound by metal, metal hydride needs a high temperature for the redox cycle. The amount of H2 released at low temperatures indicated 73.7% H2 that filled the porous, while 26,3% at high temperatures, 300°C or more, indicated H2 released from metal hydrides with redox reaction. Regarding the feasibility of operational energy saving, H2 adsorption was done at room temperature, and H2 desorption was conducted at low temperature, 85°C. Adsorption-desorption cycles of H2 were examined for their stability as H2 storage, and it was shown that at the 5th cycle, desorption of H2 decreased by 6.3% and, afterward, was nearly stable.
No takes yet. Share an insight, caveat, or question.
Harwanto et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: