Elucidates the anticoking mechanism of Ni/γ-Al₂O₃ catalysts in dry reforming of methane, implying enhanced catalyst design.
Dry reforming of methane (DRM) holds significant potential for converting greenhouse gases (CH₄ and CO₂) into synthesis gas. However, its application is severely limited by severe deactivation of Ni-based catalysts due to coking. This study systematically investigates the micromechanisms of the DRM reaction on Ni₉/γ-Al₂O₃(110) catalysts using density functional theory (DFT) calculations and microkinetic simulations. Results indicate that CH₄ dissociation preferentially occurs on the surface of Ni nanoparticles, while CO₂ activation and coke removal are dominated by the metal-support interface. The energy barrier for CO₂ hydrogenation at the interface is significantly lower than that for direct dissociation, and the key decarbonation step (C* + O* → CO) exhibits a markedly reduced barrier of 0.64 eV, effectively suppressing coke formation. Microkinetic simulations further reveal that CO is primarily generated via the CHO decomposition pathway, with the rate-determining step dynamically shifting from CO₂ hydrogenation to surface decarbonization as temperature increases. Additionally, negative external electric fields universally reduce energy barriers across key steps. This study elucidates the anticoking mechanism of Ni/γ-Al₂O₃ catalysts at the atomic scale, providing crucial theoretical foundations for rationally designing highly efficient and stable DRM catalysts.
No takes yet. Share an insight, caveat, or question.
Lv et al. (2026) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: