Plasma-enhanced deposition improved wurtzite GaN quality on sapphire, suggesting less impurity presence.
This paper demonstrates the deposition of GaN on c-plane sapphire by plasma-enhanced atomic layer deposition (PE-ALD) at 250 °C using triethylgallium and forming gas (95% N2, 5% H2) plasma. The films exhibit a wurtzite crystal structure with a full-width at half maximum of 0.31° for the (0002) peak via x-ray diffraction and an abrupt GaN–sapphire interface confirmed by scanning transmission electron microscopy. X-ray photoelectron spectroscopy and secondary-ion mass spectrometry reveal carbon and oxygen concentrations of 1 at. % and less than 3 at. %, respectively. Transfer length method analysis demonstrates a sheet resistance of 1.37 × 108Ω/□. These results provide an understanding for the low-temperature PE-ALD growth of GaN with high crystalline fidelity and minimized impurity incorporation.
No takes yet. Share an insight, caveat, or question.
Talli et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: