Evaluates adhesive strength in dissimilar joints, showing that Al/CFRP joints have higher strength than Al/Al joints.
In this study, the adhesive strength of the dissimilar joints with a polymer agent was evaluated using the laser spallation technique. The similar and dissimilar material joint samples were prepared with Al plate and unidirectional CFRP plate in the shape of a lap-joint type. The thickness of the adhesive layer was 0.05 mm. Weak bond Al/Al joint sample was prepared by applying a release agent on the adhesive surface. These samples were submitted to the shear-tensile and laser spallation tests. The spallation test could evaluate adhesive strength without stress concentration at the adhesive edge, which occurred in the shear-tensile test. In particular, the average tensile strength of Al/Al joints was 23.2 MPa, while that of Al/CFRP joints exceeded 36.5 MPa. In both Al/Al and Al/CFRP specimens, delamination occurred at the aluminum/adhesive interface. However, higher strength was estimated for Al/CFRP joints by both tests.
No takes yet. Share an insight, caveat, or question.
NANJO et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: