Answers are grounded in this paper and cite their sources.
Study demonstrates enhanced thermoelectric performance in BiSnSe films through post-selenization treatments, suggesting effective optimization methods.
In this study, we have synthesis, structural, and thermoelectric characterization of BiSnSe thin films to post-selenization treatments of varying durations (30, 60, 90, 120, and 150 min). X-ray diffraction analysis revealed that grown films crystallize in the BiSnSe phase. Post-selenization enhances the crystallinity, reduces micro-strain, and increases crystallite size, with the 120 min treated film achieving the largest crystallites (44 nm) and lowest micro-strain (1.6 × 10 -3 ). Scanning electron microscopy confirms grain growth and improved surface uniformity with selenization, reducing defects and voids. Hall effect measurements show that post-selenization increases the charge carrier concentration from 1.8 × 10 18 cm -3 (as-grown) to 5.1 × 10 18 cm -3 and enhances mobility from 20 cm 2 V -1 s -1 to 36 cm 2 V -1 s -1 (120 min). Consequently, the electrical conductivity and Seebeck coefficient are significantly improved, reaching 118 Scm -1 and 246 µV/K at 550 K, respectively, for the 120 min film. The corresponding thermoelectric power factor achieves a maximum of 5.38 µWcm -1 K -2 , highlighting the optimal selenization duration. The study demonstrates that post-selenization effectively optimizes structural, morphological, and electronic properties, providing a viable route for enhancing the thermoelectric performance of BiSnSe thin films.
No takes yet. Share an insight, caveat, or question.
Almalki et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: