Answers are grounded in this paper and cite their sources.
Research reveals fluorine doping reduces defects and improves performance in sodium-ion battery cathodes, suggesting efficient designs for energy storage.
The NASICON‐type Na 3 VAl(PO 4 ) 3 (NVAP) cathode has garnered extensive attention owing to its robust thermodynamic stability and high operating voltage enabled by multi‐electron redox reactions (V 3+ /V 4+ /V 5+ ). However, the voltage hysteresis observed in the high‐voltage region (∼4 V vs. Na + /Na), caused by derived anti‐site defects (DASDs) where V 5+ occupies Na1 vacancies (V/Na), results in sluggish Na + diffusion kinetics and poor electrochemical reversibility. To mitigate this issue, we introduced highly electronegative F doping into the NVAP structure. Density functional theory (DFT) calculations of ion migration energetics reveal that Na 2.88 VAl(PO 3.96 F 0.04 ) 3 (NVAP‐F) exhibits a higher formation energy for V/Na anti‐site defects and a higher migration barrier for V 5+ moving to the Na1 site (3.80 eV) compared to NVAP (3.15 eV). In situ XRD results further demonstrate that the F doping effectively suppresses the formation of V/Na anti‐site defects in NVAP‐F, thus alleviating voltage hysteresis during the V 4+ /V 5+ redox reaction and maintaining a low volume strain of 4.62%. Consequently, NVAP‐F delivers superior rate capability (54.4 mAh g −1 at 30 C) and exceptional long‐cycle stability (91.5% capacity retention after 5000 cycles). Comprehensive in‐/ex situ analyses confirm enhanced ion/electron diffusion kinetics in the NVAP‐F cathode. This work offers valuable insights for the development of high‐voltage and high‐rate vanadium‐based phosphate cathodes.
No takes yet. Share an insight, caveat, or question.
Shi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: