This is the authors' abstract. We don't add key points for this paper.
• NiTi with 59–70% porosity was obtained by self-propagating high-temperature synthesis. • NiTi contains austenitic B2 TiNi, martensitic B19′ TiNi, and a secondary Ti 2 Ni phase. • SHS-NiTi samples with different porosity were tested by uniaxial compression. • 11% increase in NiTi porosity reduced the yield and tensile strength by a factor of 2. NiTi samples with 59–70% porosity were obtained by the self-propagating high-temperature synthesis (SHS) using Ti, Ni, and NiTi powders as inert. The maximum and average pore sizes increase, while the maximum and average dimensions of the bridges decrease with porosity, controlled by adjusting the amount of inert additives, based on the surface and cross-sectional microscopy studies. The phase composition of porous NiTi was determined by X-ray diffraction. The alloy contains an austenitic B2 TiNi phase, a martensitic B19′ TiNi phase, and a secondary Ti 2 Ni phase. SHS-NiTi samples with different porosity were tested by uniaxial compression, revealing mechanical properties’ dependence on porosity. It is shown that with an 11% increase in the NiTi alloy porosity, the yield and compressive strength are reduced by almost a factor of 2.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Baigonakova et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: