Soft magnetic composites (SMCs) made of amorphous powder typically result in low densities due to the brittleness of the amorphous, thereby providing poor magnetic properties. For this reason, this work focuses on mixing the particle sizes of amorphous powders to increase the packing, and therefore the compact density and magnetic properties. Enhanced packing density is obtained by mixing particle size fractions of 20–45 μm and 0–10 μm in a proportion of 73:27 vol%, respectively. Properties of the SMC made from the mixed fractions are compared with those made from each fraction using an Fe-Co composition ((Fe 0.425 Co 0.30 Si 0.125 B 0.15 ) 96.5 Nb 3 Cu 0.5 ). The mixing of fractions shows an increase of 10 % in density, thus reducing interparticle voids and enhancing magnetic saturation and permeability. By contrast, lower power losses are provided by the SMC fabricated with the 0–10 μm fraction due to lower eddy currents. A comparative study on magnetic properties and power losses of SMCs made from the mixed fractions for four compositions reveal that highest permeability (μ’ = 34.5) is achieved with composition (Fe 0.46 Co 0.30 Si 0.09 B 0.10 P 0.05 ) 96.5 Nb 3 Cu 0.5 and lowest power losses at high frequency (3437 mW/cm 3 at 1 MHz and B = 50 mT) with Fe 72.5 Si 12.5 B 15 after annealing and subsequent resin infiltration. • New amorphous-base Soft Magnetic Composites. • Particle size mixing and SMC density optimisation. • Increased magnetic saturation and permeability. • Dependence of particle size and composition on power losses. • Very low power losses and stable permeability up to a frequency of 1 MHz.
No takes yet. Share an insight, caveat, or question.
Muñoz et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: