The Y₃Al₂Ga₃O₁₂:Ce³⁺-Cr³⁺ compound is one of the brightest persistent phosphors, but its persistent luminescence duration is not so long because of the relatively shallow Cr³⁺ electron trap. To compare the vacuum referred binding energy of the electron trapping state by Cr³⁺ and lanthanide ions, we selected Yb³⁺ as a deeper electron trapping center. The Y₃Al₂Ga₃O₁₂:Ce³⁺-Yb³⁺ phosphors show Ce³⁺:5d → 4f green persistent luminescence after blue light excitation. The formation of Yb²⁺ was confirmed by the increased intensity of absorption due to Yb²⁺:4f-5d at 585 nm during the charging process. This result indicates that the Yb³⁺ ions act as electron traps by capturing an electron. From the thermoluminescence glow curves, it was found that the Yb³⁺ trap makes a much deeper electron trap with a 1.01 eV depth than the Cr³⁺ electron trap with a 0.81 eV depth. This deeper Yb³⁺ trap provides a much slower detrapping rate of filled electron traps than the Cr³⁺-codoped persistent phosphor. In addition, by preparing transparent ceramics and optimizing Ce³⁺ and Yb³⁺ concentrations, the Y₃Al₂Ga₃O₁₂:Ce³⁺(0.2%)-Yb³⁺(0.1%) as-made transparent ceramic phosphor showed super-long persistent luminescence for over 138.8 h after blue light charging.
No takes yet. Share an insight, caveat, or question.
Ueda et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: