Er3+:Ca9La(VO4)7 crystal with dimensions of φ24×22 mm3 has been successfully grown by the Czochralski method. The spectral properties of Er3+:Ca9La(VO4)7 crystal were investigated. The oscillator strength parameters Ωt (t = 2, 4 and 6) in Er3+:Ca9La(VO4)7 crystal were calculated to be: Ω2 = 9·05×10−20 cm2, Ω4 = 3·34×10−20 cm2 and Ω6 = 2·1×10−20 cm2 for π‐polarisation and Ω2 = 23·88×10−20 cm2, Ω4 = 3·92×10−20 cm2 and Ω6 = 1·89×10−20 cm2 for σ‐polarisation. The emission cross‐sections σem for π‐polarisation and σ‐polarisation at 1534 nm are 0·98×10−20 and 1·23×10−20 cm2 respectively. The fluorescence lifetime and radiative lifetime of the 4I13/2→4I15/2 transition are 3·93 and 2·69 ms respectively. These results show that Er3+ doped Ca9La(VO4)7 crystals may be regarded as 1·55 μm laser gain medium materials.