The thermal degradation mechanism of LixNi1.02O2 and LixNi0.89Al0.16O2 (x = 0.50 and 0.30) was studied by in situ X-ray diffraction correlated with thermal gravimetric analysis coupled with mass spectrometry. The degradation mechanism appears to be the same for both types of samples. It consists of two steps: the first step, corresponding to the lamellar to pseudo-spinel transformation, is accompanied by an oxygen loss only for compounds with an initial (Li + M)/O ratio (M = Ni, Al) smaller than 3/4. The second step corresponds to the progressive transformation to a NiO-type structure, with an oxygen loss for both initial lithium compositions. The thermal stabilization obtained by partial aluminum substitution for nickel can be explained by the stability of the Al3+ ions in tetrahedral sites, which disrupts the cationic migrations necessary for the phase transformations observed upon increasing temperature to occur.
No takes yet. Share an insight, caveat, or question.
Guilmard et al. (2003) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: