Answers are grounded in this paper and cite their sources.
Directional solidification evaluates machinability in Al-Si and Al-Si-Bi alloys, suggesting Bi improves performance.
This work investigates the effects of growth rate (GR), cooling rate (CR) and eutectic microstructure on the machinability of Al-12.6Si and Al-12.6Si-3.2Bi (wt.%) alloys. Directional solidification experiments were performed using a water-cooled upward solidification apparatus, enabling a range of GR and CR values along the length of the ingots. The as-solidified microstructures consisted of primary α-Al dendrites and interdendritic eutectic Si, while the Bi-containing alloy exhibited additional Bi globules dispersed within the eutectic regions. Machinability was evaluated based on maximum cutting temperature ( T max ), heating rate (HR) and tool flank wear (Vb max ). In the binary alloy, CR and eutectic spacing ( λ Si ) had negligible influence on T max , which remained approximately constant at 46 °C. On the other hand, the ternary alloy exhibited T max values ranging from 50 to 63 °C. Higher HR values were associated with higher CR and finer λ Si for both alloys. Although Bi addition did not significantly affect HR, it promoted the formation of built-up edge (BUE), which contributed to a higher T max . The addition of Bi improved machinability by reducing Vb max by nearly 40% compared with the binary alloy.
No takes yet. Share an insight, caveat, or question.
Rocha et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: