Methodological study reveals improved precision of specified area under band analysis in polyolefins, suggesting superior tracking of plastic degradation during accelerated aging.
The current measurement techniques described in the literature for the determination of the carbonyl index (CI) for polyolefins such as polyethylene and polypropylene were compared and contrasted. These were all found to be inconsistent or inaccurate and were not capable of differentiating significant changes in carbonyl peak evolution throughout accelerated ageing. As a consequence of these findings, a methodology, specified area under band (SAUB) is presented here to more accurately represent the CI as a general means of reporting. The increased precision in the methodology is explained and compared to other methodologies for determining CI. The SAUB method is also shown to be capable of elucidating the differences in relative extent and rates of CI for different polyolefins, exposed to the same conditions over the same time period.
No takes yet. Share an insight, caveat, or question.
Almond et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: