Answers are grounded in this paper and cite their sources.
Investigates post-processing effects on mechanical behavior in nickel-based superalloys, indicating critical methods for improvement.
Powder bed fusion–laser beam (PBF-LB) is a primary metal additive manufacturing (AM) process for industrialization. However, post-processing recipes for PBF-LB are distinct from those of conventional manufacturing and remain critical in governing the mechanical performance of PBF-LB components. This study investigates the influence of post-processing on the mechanical behaviour of Haynes 282—a Nickel-based superalloy utilized in turbine exhaust case and other high-temperature (up to 760 °C) applications—fabricated using high productivity themed PBF-LB with layer thickness of 60 and 90 μ m. The as-built condition and recipe with solution treatment at 1150 °C (conventional treatment) exhibited anisotropy in both grain morphology and mechanical performance. Increasing the solution Treatment temperature to 1200 °C successfully reduced anisotropy in the 60 μ m layer thickness build, owing to partial recrystallization, however anisotropy still exists in the 90 μ m layer thickness build. Solution treatment at 1250 °C resulted in complete recrystallization and isotropic hot ductility across both the builds, albeit with a significant reduction in strength. These microstructural and mechanical response variations are discussed with emphasis on layer thickness, the volumetric energy density, dislocation density in the as-built microstructures, and solution treatment temperatures.
No takes yet. Share an insight, caveat, or question.
Swaminathan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: