Substantially reduced energy and power capabilities of lithium-ion cell operating at low temperatures pose a technical barrier for market penetration of hybrid electric vehicles and pure electric vehicles. The present work delineates Li-ion cell behaviors at low temperatures by a combined experimental and modeling approach. An electrochemical-thermal coupled model, incorporating concentration- and temperature-dependent transport and kinetic properties, is applied and validated against 2.2Ah 18650 cylindrical cells over a wide range of temperatures (−20°C to 45°C) and discharge rates. Simulation and experimental results demonstrate the dramatic effects of cell self-heating upon electrochemical performance. A nonisothermal Ragone plot accounting for these important thermal effects is proposed for the first time for Li-ion cells and more generally for thermally coupled batteries. Detailed resistance analysis indicates that performance limits at −20°C depend on not only discharge rates but also thermal conditions. Optimization of cell design parameters and material properties is performed for 1 C rate discharge starting from −20°C, where the principal performance limitations are found to be Li+ diffusion in the electrolyte and solid-state Li diffusion in graphite particles, instead of charge-transfer kinetic or ohmic resistance.
No takes yet. Share an insight, caveat, or question.
Ji et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: