Synthesis of fibers from waste high-impact polystyrene (HIPS) have been successfully done using electrospinning method. The HIPS solutions were made with a single solvent (DMF or d-limonene), a mixed solvent (d-limonene/DMF), and with the addition of acetone to the previously stated solvents. The effects of HIPS concentration, a mix of solvent, and the addition of acetone on the morphology and the diameter of fibers were observed. The morphological change from particles to fibers took place along with the increasing concentration of HIPS in d-limonene. For other precursor solutions using DMF solvent, bead free fibers could be obtained even at low levels. The average diameter of fibers increased along with the increase of the HIPS concentration in DMF. At the concentrations of 15, 20, 25, 30, and 35 wt.%, the average diameters were 1.85, 2.09, 2.66, 3.59, and 7.38 μm, respectively. For the precursor solutions with the combination of different solvents (HIPS/DMF), the existence of beads was influenced by the ratio of solvents. When the ratio of d-limonene/DMF was 75:25, the obtained beaded fibers had a relatively large amount of beads. At the ratio of 50:50, fewer beads were found. Bead-free fibers were finally reached when the ratio of HIPS / DMF was 25:75. The addition of acetone reduced the diameter of the produced fibers. However, too much addition of acetone caused the fibers to be wet. Additionally, the diameter became larger if the addition of acetone surpassed a certain amount of volume.
No takes yet. Share an insight, caveat, or question.
Zulfi et al. (2017) studied this question.
Synapse has enriched 4 closely related papers on similar clinical questions. Consider them for comparative context: