Answers are grounded in this paper and cite their sources.
This thesis examines the melt ejection mechanisms in laser drilling, highlighting their dependence on multiple parameters.
This thesis aims to investigate the rear melt ejection of long pulse laser drilling to further the understanding of the melt ejection mechanism and its unpredictable change with various different parameters including, assist gas pressure, laser power, pulse width, beam profile and material type, as well as to provide a clearer understanding of the relationship between these variables and the rear ejecta cloud and its evolution with time. To do this, modern high-speed filming technology has been combined with advanced image processing and particle tracking programs which have been developed specifically to analyse the rear melt ejection of laser drilling. These techniques have proven successful in analysing large numbers of high-speed videos and outputting large amounts of quantitative data, including particle velocities, diameters and momentums. Several interesting findings were made, including the observation of three main ejection mechanisms, the central fast jet, the initial jet and radial ejection. The time resolved evolution of the rear ejecta cloud was found to be impacted by numerous exploding particles, across a range of different parameters. Ten frequently occurring archetypal shapes were identified for the rear ejecta cloud, giving an insight into how it changes with respect to different parameters. Also, a strong material dependence was found to impact particle number, velocity, diameter and momentum when comparing mild steel, titanium and aluminium. The results showed that as well as material type, mean velocity was dependent on assist gas pressure but showed little change with laser power. Across all parameters tested, mean velocity was observed between 4 - 15 ms^-1, whilst maximum velocity is expected to be in excess of 90 ms^-1. Mean particle diameter was shown to be dependent on both assist gas pressure and material type, but was also found to have no clear trending relationship to laser power, however variation of up to 50 μm was observed. Across all parameters, mean particle diameter shown to be 200 - 500 μm, with a maximum diameter of up to 1700 μm. Through all parameters tested, it was apparent that the majority of particles had relatively low momentums for each individual set of results and that the majority of particles were both relatively small and slow through all parameters tested. Differing trends were observed between a 2kW IPG 2000S fibre laser and a 6kW QCW IPG fibre laser, which were both used in single pulse mode, due to a difference in beam profile and nozzle size. As assist gas pressure was increased, particle number increased for the 2kW laser used but decreased for the 6kW laser used. Also, for the mild steel and aluminium results, when laser power increased, particle number increased for the 2kW laser but decreased for the 6kW laser. Overall, this work provides a new insight into the long pulse laser drilling melt ejection mechanism and the rear melt ejection process. Future work hopes to further make use of the techniques used in this project to develop on the understanding of the rear particle ejecta cloud and shed further light on newly discovered trends.
No takes yet. Share an insight, caveat, or question.
Connor Jones (2020) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: