Answers are grounded in this paper and cite their sources.
Paper-related production of composite materials from Al 2 O 3 -pre-composite powder (NiAl–10 wt pct Al 2 O 3 ). PPS allowed for forming ceramic–intermetallic composites. MA produced the pre-composite powder. Six series of composites were made, differing in temperature (1200 °C, 1300 °C, 1400 °C) and content of pre-composite powder (2.5 and 5 wt pct with respect to the amount of Al 2 O 3 ). Highest hardness was obtained for composite series sintered at 1300 °C. Both series, with various pre-composite powder content, had a value of 20.8 to 20.9 GPa. Samples containing 2.5 wt pct pre-composite powder sintered at 1200 °C were highest K IC value of 4.72 ± 0.34 MPa·m 0.5 . Interestingly, the same value was obtained in composites containing 5 wt pct pre-composite powder sintered at 1300 °C. For both series with different pre-composite powder content, sintering at 1400 °C obtained the highest strength. For composites containing 2.5 wt pct pre-composite powder, splitting tensile strength value was 255.98 MPa, while for samples with 5 wt pct, pre-composite powder was 264.01 MPa Graphical Abstract
No takes yet. Share an insight, caveat, or question.
Zygmuntowicz et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: