Answers are grounded in this paper and cite their sources.
This study investigated the influences of water-to-binder mass ratio (0.44, 0.47, and 0.50), and waterglass (8%, 12% and 16%) and fly ash (0%, 25% and 50%) contents on the slump, cubic compressive strength, and static and dynamic compressive behaviors of slag-based geopolymer concrete (GC). Static compressive tests were carried out by using an electro-hydraulic servo-controlled compressive test system, and dynamic ones were performed by using a split Hopkinson pressure bar (SHPB) apparatus. The specimens with a wide range of the compressive strength (from 50 MPa to 80 MPa) were prepared. The results show that the workability of fresh slag-based GC increased with increasing water-to-binder ratio, and waterglass and fly ash contents. The cubic compressive strength increased with the decreases of water-to-binder ratio and fly ash content, and the increase of the waterglass content. Increasing waterglass content contributed to the improvement of the static compressive behavior of slag-based GC, such as elastic modulus and peak stress, while it led to the rise of the brittleness. Slag-based GC with different water-to-binder mass ratios, and waterglass and fly ash contents showed a strong strain-rate dependency. However, the inclusion of 50% fly ash induced a sharp increase of the dynamic compressive strength and dynamic increase factor (DIF) at a high strain rate. Moreover, both the two formulations for fitting static compressive stress-strain curve and DIF with higher accuracy were proposed in this study.
No takes yet. Share an insight, caveat, or question.
Ou et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: