Tin-based anodic materials, benefiting from their large theoretical specific capacity and minimal operating potential, are considered high-development potential alternative anodes for lithium-ion batteries (LIBs). Nevertheless, the alloying-dealloying processes between tin (Sn) and lithium ions result in severe volume expansion, which leads to a poorly stabilized solid-electrolyte interface (SEI) layer and resultant inferior cycling performance, posing major obstacles to their commercialization. Herein, a structural regulation strategy was proposed to optimize the interstitial void buffer layer within yolk–shell structures to mitigate the lithiation-associated volume expansion. The tetraethyl orthosilicate-hydrolyzed SiO2 layer was located between Sn and the resin-derived carbon coating, whose thickness could be sophisticatedly optimized via regulating the hydrolysis durations. Following the carbonization and etching, an optimized buffer layer was encapsulated within a protective carbon shell (Sn@Void@C), which could effectively accommodate Sn’s volume expansion during the alloying period, significantly enhancing its performance in electrochemical processes and structural stability. Specifically, the Sn@Void@C anode retained a high specific capacity of 720 mAh g–1 after 400 cycles at 0.2 C and demonstrated an outstanding capacity of 520 mAh g–1 after 500 cycles at 0.5 C. This work provides a facile and effective strategy for rationally designing tin-based anodes for lithium-ion batteries.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Zhao et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: