A stretchable Li4 Ti5 O12 anode and a LiFePO4 cathode with 80% stretchability are prepared using a 3D interconnected porous polydimethylsiloxane sponge based on sugar cubes. 82% and 91% capacity retention for anode and cathode are achieved after 500 stretch-release cycles. Slight capacity decay of 6% in the battery using the electrode in stretched state is observed.