Investigates resistance spot welding impacts on microstructure and mechanical properties in dissimilar steel sheets, suggesting optimization is crucial.
This study investigates the resistance spot welding behavior of dissimilar low-carbon CR3 steel and coated transformation-induced plasticity-aided bainitic ferrite (TBF) steel sheets widely used in automotive body applications. The effects of welding current (6-7-8-9 kA) and welding time (240–400 ms) on weld microstructure, nugget size, indentation depth, and mechanical performance were systematically examined. Metallographic analysis revealed no macroscopic weld defects; however, limited mixing was observed in the fusion zone, particularly at lower heat inputs. Increasing heat input enhanced material mixing and widened the heat-affected zone (HAZ), especially on the TBF side, but also promoted liquid metal embrittlement (LME)-induced surface microcracks associated with Zn-coating penetration along grain boundaries. The maximum nugget size reached 8.34 mm at 9 kA–400 ms, while the indentation depth remained within automotive acceptance limits, with a maximum value of 21.65%. Tensile-shear tests showed that all fractures occurred in the HAZ of the thinner CR3 sheet in a tearing mode, with a maximum failure load of 4.25 kN at 7 kA–240 ms. Despite the presence of microcracks in the TBF HAZ, the joint strength was governed by the lower-strength CR3 sheet. The results highlight the importance of optimized welding parameters to balance sufficient nugget growth and minimize LME susceptibility in dissimilar advanced high-strength steel (AHSS)–mild steel combinations.
No takes yet. Share an insight, caveat, or question.
İmren Öztürk Yılmaz (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: