Answers are grounded in this paper and cite their sources.
Evaluating TeO2 vitrification enhances management of LiCoO2 in lithium batteries, indicating a sustainable approach.
The making of glasses using LiCoO 2 as electrode-active material from Li + -ion batteries and TeO 2 as glass former is reported. The reagents were mixed guided by the x LiCoO 2 -(100 – x )TeO 2 with x = 20, 30, 40 and 50 mol% formulas and melted at 950 °C for 15 min. The obtained materials were then characterized by density, X-ray diffraction (Mo- K α radiation), Fourier-transform infrared (FT-IR) spectroscopy, and differential scanning calorimetry (DSC). The products appeared X-ray amorphous up to 40 mol% LiCoO 2 , whereas at 50 mol% LiCoO 2 the formation of a glass-ceramic was indicated. The FT-IR spectra harmonized with the occurrence of TeO 3+1 , TeO 4 and TeO 3 units, and a conversion toward the latter with increasing LiCoO 2 content. The DSC analysis exposed that the glass transition and crystallization temperatures overall tended to decrease with increasing LiCoO 2 content, thus leading to reduced glass stability. The evaluation overall supports the fitness of TeO 2 for LiCoO 2 vitrification at moderate loading, thus encouraging additional research with material recovered from spent batteries. • Tellurite glasses made using LiCoO 2 electrode-active material and TeO 2 as glass former • Characterized by density, XRD, FT-IR, and DSC • Vitrification with TeO 2 suggested as strategy for management of lithium battery electrode
No takes yet. Share an insight, caveat, or question.
José A. Jiménez (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: