Answers are grounded in this paper and cite their sources.
Investigates enhanced adhesion and mechanical properties in dental composites using core-shell fibers, implying improved material performance.
This study investigates core–shell electrospun fibers with a polyacrylonitrile (PAN) core and a poly(methyl methacrylate) (PMMA) shell incorporating tri(ethylene glycol) dimethacrylate/bisphenol A glycidyl methacrylate (TEGDMA/BisGMA) resin. The objective is to enhance interfacial adhesion between the fibers and dental resin, ultimately improving mechanical properties. The coaxial electrospinning technique was used to produce the fibers (PAN‐PTB), which were introduced into a resin matrix at various mass fractions. Extraction experiments indicated that the fibers contained 22.0% TEGDMA/BisGMA, which is close to the theoretical value of 26.3%. Tensile testing of the fiber mats revealed that the PMMA mat exhibited significantly inferior tensile properties when compared to the PAN mat, with a 72.0% reduction in tensile strength and a 74.4% decrease in work at break. In contrast, the PAN‐PTB mat demonstrated a remarkable enhancement in tensile strength, modulus, elongation at break, and work of rupture, with increases of 239.2%, 72.0%, 105.4%, and 707.3%, respectively, compared to the PAN mat. The optimal flexural properties were achieved with composites reinforced by 2.5 wt% PAN‐PTB fibers, which had about 0.6 wt% PAN, resulting in a 16.3% enhancement in flexural strength compared to neat resin. Despite lower PAN content than in composites with 2.5 wt% neat PAN fibers, the two types of composites did not show significant differences, owing to the PTB fiber shell, which enhanced interfacial adhesion. Microscopy analysis confirmed strong adhesion of PAN‐PTB fibers with the matrix, with no visible interfacial gaps.
No takes yet. Share an insight, caveat, or question.
Shekarian et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: