The effect of uniaxial stress on the one-phonon Raman lines of CdS having A₁, E₁, and E₂ symmetries are studied for compressive force →F, either along the a axis (^x) or the c axis (^z) and using a low-temperature stress cryostat. The scattering geometries chosen resulted in the phonon propagation direction →q being either parallel or perpendicular to z; this in turn allowed the observation of pure E₁(TO), E₁(LO), A₁(TO), and A₁(LO) lines. For →F∥^x, the lines or their components shift linearly with stress. The E₂ line at 256 cm^-1 splits into two clearly resolved components, the polarization features being consistent with the deformation-potential theory. The E₁(TO) and the E₁(LO) lines separate further, whereas the A₁(TO) and the A₁(LO) lines increase at the same rate. For →F∥^z, all the lines exhibit shifts linear in stress; the E₁(TO) and the E₁(LO) lines increase at the same rate, and the E₂ line at 256 cm^-1 does not split. From the results for →F∥^x and →F∥^z, the deformation-potential constants characterizing each line have been deduced. A comparison of the piezospectroscopy of the doubly degenerate E₁ line of CdS with that of the E lines of α-quartz is presented along with some new results for the latter. The LO overtones observed in ȳ(zz)y geometry shift linearly for →F∥^z, the rates of shift increase linearly with increasing order. The magnitudes of these shifts suggest that all overtones are of E₁ nature.
No takes yet. Share an insight, caveat, or question.
Briggs et al. (1976) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: