SiC ceramics were fabricated by spark plasma sintering technique with the use of Al2O3 additive. The sintering process was carried out at three dierent temperatures in the range of 17001800 C applying two dierent pressures 40 and 80 MPa under vacuum atmosphere. The eect of additive, dierent temperatures and pressures on densication behaviour, density, Vickers hardness, fracture toughness, and microstructure were examined. The hardness and fracture toughness of the samples were evaluated by the Vickers indentation technique. Microstructure of spark plasma sintered SiC samples were characterized by using scanning electron microscopy technique. The highest value of fracture toughness 5.9 0.2 MPa m 1/2 was achieved with the addition of 5 vol.% Al2O3.