Most piezoelectric power generators rely on polycrystalline perovskite oxide thin films fabricated at high temperatures. Here, we report the direct room-temperature deposition of amorphous Pb(Zr,Ti)O3 thin films onto a polymer substrate, enabling efficient bending-driven power generation. Regulation of chemical states via oxygen partial pressure during sputter deposition was crucial for inducing dipolar polarization arising from locally oriented TiO6 octahedra at the short-range scale. The resulting amorphous films exhibited peak output voltage, power, and power density of approximately 40.4 V, 480 μW, and 3.01 × 106 μW cm–3, respectively, surpassing values reported for conventional polycrystalline oxide thin-film cantilevers within our knowledge. The excellent figure of merit of the energy harvester reflects a trade-off between piezoelectric response and relative permittivity. The optimized device further exhibited robust physiological sensing capabilities, highlighting the extended potential of the amorphous thin films for other functional applications.
No takes yet. Share an insight, caveat, or question.
Han et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: