This is the authors' abstract. We don't add key points for this paper.
A reliable and reproducible deposition process for the fabrication of Al 2 O 3 waveguides with losses as low as 0.1 dB/cm has been developed. The thin films are grown at ~ 5 nm/min deposition rate and exhibit excellent thickness uniformity within 1% over 50times50 mm 2 area and no detectable OH - incorporation. For applications of the Al 2 O 3 films in compact, integrated optical devices, a high-quality channel waveguide fabrication process is utilized. Planar and channel propagation losses as low as 0.1 and 0.2 dB/cm, respectively, are demonstrated. For the development of active integrated optical functions, the implementation of rare-earth-ion doping is investigated by cosputtering of erbium during the Al 2 O 3 layer growth. Dopant levels between 0.2-5times10 20 cm -3 are studied. At Er 3+ concentrations of interest for optical amplification, a lifetime of the 4 I 13/2 level as long as 7 ms is measured. Gain measurements over 6.4-cm propagation length in a 700-nm-thick Al 2 O 3 :Er 3+ channel waveguide result in net optical gain over a 41-nm-wide wavelength range between 1526-1567 nm with a maximum of 5.4 dB at 1533 nm.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Wörhoff et al. (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: