Answers are grounded in this paper and cite their sources.
Experiments and calculations are used to determine the optimum parameters of the peroxide delignification of larch wood in the presence of MnSO4 catalyst that provides high yields of cellulose (44.3 wt %) with low residual lignin contents at a temperature of 100°C, an H2O2 content of 6 wt %, a CH3COOH content of 25 wt %, a LWR of 15, and a duration of 3 h The cellulose obtained under optimum conditions has a chemical composition of cellulose, 92.7 wt %; lignin, 0.6 wt %; and hemicellulose, 5.7 wt %. IRS and X-ray diffraction are used to determine that cellulose obtained from larch wood has a structure similar to that of industrial microcrystalline cellulose. The proposed catalytic approach allows cellulose to be obtained from larch wood with a minimal lignin content under mild conditions in one step and with a high yield, a degree of crystallinity of 0.8, and a crystallite size of 3.0 nm.
No takes yet. Share an insight, caveat, or question.
Sudakova et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: