dispersoids during heating to homogenization temperature and homogenization of the alloys, and during isothermal heat treatments of the as-cast alloys (T5 temper). The highest hardness of Sc and (Sc + Y) modified alloys was attained by heat-treating alloys in the as-cast state in the temperature range between 350 °C and 450 °C (via T5 temper).