Investigates interface stability of coated cathodes, indicating improved performance in lithium-ion batteries.
Solid polymer electrolytes (SPEs) are suitable electrolytes for enhancing the safety of lithium‐ion batteries (LIBs). However, PEO‐based SPEs undergo oxidative decomposition when in contact with 4 V‐class cathodes due to their narrow electrochemical window. In this study, we investigated the effect of LiNbO 3 or Nb 2 O 5 layers on the stability of the SPE/LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) interface. A coated electrode was fabricated by deposition of coating materials on a single‐crystalline‐like NMC622 electrode sheet using radio frequency magnetron sputtering. The resistance at the SPE/NMC622 interface, R NMC of the non‐coated NMC622 increased significantly over time, suggesting the formation of a large resistance layer at the PEO/NMC622 interface at 4.2 V. For coated NMC622, the increase rate of R NMC was lower compared to non‐coated NMC622. Particularly when the coating thickness was ca. 300–400 nm, R NMC for both coated electrodes showed little change over time, maintaining its initial value. This suggests that a highly stable SPE/NMC622 interface is formed even at a potential of 4.2 V. However, a gradual decrease in capacity was observed with repeated cycles for LiNbO 3 ‐coated NMC622. This was attributed to the higher instability of the LiNbO 3 coating at high potentials compared to the Nb 2 O 5 coating.
No takes yet. Share an insight, caveat, or question.
SAHASHI et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: