Answers are grounded in this paper and cite their sources.
Half-micron-thick tungsten oxide films were deposited by the sol−gel method onto indium tin oxide (ITO) coated soda lime silicate substrates. Following a 100 °C prebake, the samples were fired with a carbon dioxide laser at a variety of power densities and translation speeds. The laser-fired tungsten oxide films were characterized by spectrophotometry, electrochemistry, multiangle ellipsometry, and transmission electron microscopy and compared to similar furnace-fired films. The data showed an increase in electrochromic response with increased firing temperature up to the point where crystallization of the tungsten oxide retarded electrochromic response. A window with graded electrochromic properties was made by laser firing.
No takes yet. Share an insight, caveat, or question.
Taylor et al. (1996) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: