Combined in situ X-ray absorption near-edge structure (XANES) and extended X-ray absorption fine structure (EXAFS) studies have been conducted to follow gold structural changes of low-content (<1%Au) gold-ceria catalysts in water-gas shift (WGS) reaction tests at 100 and 200 °C; and after heating the used catalysts in oxygen gas at 150 °C. Gold in the fresh (400 °C-calcined) material was atomically dispersed in cerium oxide. Under WGS reaction conditions, reduction of the oxidized gold species was observed, accompanied by gradual gold aggregation. The Au−Au coordination number is zero for the fresh material, but increases with the reaction temperature, to 6.5 ± 2.4 (after use at 100 °C) and to 8.7 ± 1.5 (after 200 °C) in a gas mixture containing 5% CO- 3% H2O in helium. The second important parameter is the reaction gas composition which determines the extent of Au−O reduction. The lower the reduction potential of the reaction gas mixture, the more oxidized the gold is in the used catalyst, and the higher its activity. The maximum activity of Au-CeO2 was that of the fully dispersed Au−O−Ce fresh material. Loss of surface oxygen took place during reaction, as measured by H2-TPR of the used samples, and it was commensurate with the activity loss. Attempts to reoxidize and redisperse the gold by heating in oxygen gas at 150 °C were not effective. However, we report here that complete recovery of the surface oxygen amount and redispersion of gold in ceria was possible after a 400 °C- oxygen treatment of both the 100 °C- and 200 °C- used catalyst samples, with concomitant recovery of the initial catalyst activity. These tests were conducted by consecutive H2-TPR/steady-state catalyst activity measurements in the same microreactor.
No takes yet. Share an insight, caveat, or question.
Deng et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: