Compares physico-mechanical properties of 3D-printed resins with conventional materials, indicating comparable strength but varying hardness.
Objective: To compare the physico-mechanical properties (microhardness, surface roughness, and flexural strength) of permanent 3D-printed dental resins with those of a resin nanoceramic computer-aided design and computer-aided manufacturing (CAD/CAM) block and a composite resin. Methods: Four groups were tested: composite resin (Clearfil Majesty Esthetic), resin nanoceramic CAD/CAM block (Cerasmart), and two 3D-printed resins (Saremco Crowntec, VarseoSmile Crown Plus). Disk- and bar-shaped specimens were prepared according to ISO standards. Microhardness (Vickers test), surface roughness (profilometer), and flexural strength (three-point bending test) were evaluated. Data were analyzed using analysis of variance and Tukey post hoc tests (p < 0.05). Results: Cerasmart showed the highest microhardness (85.53 ± 3.97) and flexural strength (184.45 ± 9.42), while Saremco Crowntec exhibited the lowest microhardness (38.63 ± 2.14). Clearfil Majesty had the highest surface roughness (1.24 ± 0.35). Although the measured flexural strength values of 3D-printed resins exceeded the ISO 4049 minimum threshold, several samples were close to or below the limit. Conclusions: Within the limitations of this in vitro study, 3D-printed permanent resins exhibited mechanical properties comparable to conventional restorative materials in certain parameters, although inferior hardness values were observed compared to CAD/CAM blocks. Nevertheless, the present findings should be interpreted with caution, and further long-term clinical investigations are necessary before translating these results into clinical practice.
No takes yet. Share an insight, caveat, or question.
Arıkan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: