Demonstrates reproducible growth of semiconducting vertically aligned carbon nanotube arrays via chemical vapor deposition, highlighting catalyst thickness thresholds.
The structure and morphology of vertically aligned CNT (VACNT) arrays grown by CVD on Fe–Al2O3/Si(001) substrates are studied using scanning and high-resolution transmission electron microscopy (HRTEM) methods and Raman scattering. It is established that reproducible growth of continuous VACNT arrays is achieved only if the deposited Fe layer is at least 2 nm thick, while the particle size of the catalyst formed by annealing at 700 °C varies in a range of 2-10 nm and the array consists mainly of single- and double-walled CNTs with a diameter of 1-6 nm. The Raman spectrum is characterized by the presence of a radial breathing mode in the region 95-232 cm–1 and an intense G mode that is split into peaks at 1594 cm–1 and 1568 cm–1 upon laser excitation at the wavelength λ = 785 nm. According to the literature data, both modes indicate predominantly semiconductor nature of tubes in the array. The measured surface resistance of the VACNT array is 320±20 Ω/□.
No takes yet. Share an insight, caveat, or question.
Semenova et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: