Recording performances for Ba-ferrite particulate perpendicular magnetic tapes, with different coercivity values, <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Hc⊥</tex> =470- 1930 Oe, and other properties substantially unchanged, were investigated with ring-shaped heads. Noise was found to be independent of <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Hc⊥</tex> . It was ascertained that reproduced voltages and signal-to-noise ratios were constant and highest for <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Hc⊥ > Hco⊥, Hco⊥</tex> being 600 - 700 Oe depending on recorded wavelength, and that they decreased in proportion to <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Hc⊥</tex> for <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">Hc⊥ < Hco⊥</tex> . Therefore, Ba-ferrite tapes can be designed, with their highest performances, to adjust their coercivity so as to meet ferrite or metal head recording ability.
No takes yet. Share an insight, caveat, or question.
Isshiki et al. (1985) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: