Evaluates fracture strength in endodontically treated molars, indicating material choice is crucial.
Aim: To evaluate fracture strength (FS) and failure mode (FM) of additively manufactured endocrowns fabricated from two three-dimensional-printed resin composites with distinct inorganic filler contents, tested at two intracoronal preparation depths following thermomechanical aging. Materials and Methods: Twenty-eight endodontically treated human mandibular molars were restored using additively manufactured endocrowns according to material (Bio Crown or Voxelprint) and preparation depth (3 mm or 5 mm). After adhesive cementation and thermomechanical aging (300,000 cycles; 5°C–55°C), FS was measured under axial loading (0.5 mm/min), and FM were classified into four categories. Data were analyzed by two-way analysis of variance and Tukey’s test (α = 0.05). Results: Restorative material significantly affected FS ( P = 0.0063), whereas preparation depth did not ( P = 0.403). Voxelprint showed higher FS than Bio Crown, independent of depth, with a significant difference between Voxelprint 5 mm and Bio Crown 5 mm ( P = 0.034). Preparations with greater depth were associated with a higher frequency of catastrophic vertical fractures. No interaction effect was observed. Conclusion: Resin composition influenced FS more than preparation depth. Increased depth did not improve load capacity but shifted failure toward more severe patterns.
No takes yet. Share an insight, caveat, or question.
Souza et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: