This is the authors' abstract. We don't add key points for this paper.
An Al 2 O 3 /SiO buffer layer was incorporated in a metal–insulator–semiconductor (MIS) Ta 2 O 5 capacitor for dynamic random access memory (DRAM) application. Al 2 O 3 was chosen for the buffer layer owing to its high band offset against silicon and oxidation resistance against increase in effective oxide thickness (EOT). It was clarified that post-deposition annealing in nitrogen at 800 °C for 600 s increased the band offset between Al 2 O 3 and the lower electrode and decreased leakage current by two orders of magnitude at 1 V. Furthermore, we predicted and experimentally confirmed that there was an optimized value of y in (Si 3 N 4 ) y (SiO 2 ) (1- y ) , which is 0.58, for minimizing the leakage current and EOT of SiON. To clarify the oxidation resistance and appropriate thickness of Al 2 O 3 , a TiN/Ta 2 O 5 /Al 2 O 3 /SiON/polycrystalline-silicon capacitor was fabricated. It was confirmed that the lower electrode was not oxidized during the crystallization annealing of Ta 2 O 5 . By setting the Al 2 O 3 thickness to 3.4 nm, the leakage current is lowered below the required value with an EOT of 3.6 nm.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Tonomura et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: